Pink Fused aluminum oxide F220

Pink Fused aluminum oxide is obtained by adding chromium oxide to high purity aluminum oxide during the fusion process,with high hardness,good toughness and high grinding efficiency.

$900.00 /MT

PINK FUSED ALUMINUM OXIDE F220

Chemical Composition

Pink Fused aluminum oxide F220Al2O3(%)Cr2O3(%)Na2O(%)Fe2O3(%)
Low Chromium≥98.00.2-0.45≤0.40.01-0.05
Medium Chromium≥97.80.45-1.00≤0.40.01-0.05
High Chromium≥96.51.00-2.00≤0.40.01-0.05

PSD(Particle Size Distribution) of Pink Fused aluminum oxide F220

    MESH  DIAMETER/UM  %
+140+106UM0
+200+75UM≤15%
+230+63UM*
+230+270+63UM+53UM≥40%
+230+270+325+63UM+53UM+45UM≥60%

Pink fused aluminum oxide Main Applications

1. Used for precision grinding of measuring tools, lathe main shafts, instruments and apparatus parts, threading work pieces and many other applications in grinding like flute grinding, tooth grinding, dry grinding of blade segments, tool and internal grinding and mounted point.

2. The best suitable for high alloy steel applications, ideal for tool sharpening such as high speed steel cutters, reamers, chisels, end mill and sharpening band saw blades.

3.Recommended for knife-sharpening applications, working non-ferrous metals and the alloys.

4.Good performance for vitrified bonded abrasives , vitrified grinding wheels, coated abrasives and blasting abrasives.

5.Also be used for softer materials, such as wood, Synth-etics, etc.

Packaging of Pink fused aluminum oxide

Production lines of Pink fused aluminum oxide

 

Production Sizes of Pink fused aluminum oxide

                For abrasiveF12 F14 F16 F20 F22 F24 F30 F36 F40 F46 F54 F60 F70 F80 F90 F100 F120 F150 F180 F220

#12 #14 #16 #20 #24 #30 #36 #40 #46 #54 #60 #70 #80 #90 #100 #120 #150 #180 #220

                For refractory0-1mm 1-3mm 3-5mm 5-8mm